Lugar del origen
Hunan, China
Composición Química
CuSnTi
Application 1
Cubic boron Nitride CBN,PCBN soldering
Application 2
Diamond soldering
Application 3
Alumina ceramic soldering
Application 4
Silicon carbide ceramic soldering
Application 5
Glassy graghite soldering
Solidus and liquidus line
850-880℃
Brazing temperature
880-930℃